AWS A5.18 ER70S-6 Logam Pengisi Kawat Las Baja Karbon untuk Las Arc Terlindung Gas, Kabel Padat

Katrangan singkat:

ER70S6 minangka kawat las baja entheng sing ngandhut tingkat mangan lan silikon sing luwih dhuwur tinimbang kawat MIG standar liyane kanggo ngasilake welds kualitas dhuwur nalika digunakake ing baja sing reged, berminyak, utawa teyeng.


Detail Produk

Tag produk

ER70S6 minangka kawat las baja entheng sing ngandhut tingkat mangan lan silikon sing luwih dhuwur tinimbang kawat MIG standar liyane kanggo ngasilake welds kualitas dhuwur nalika digunakake ing baja sing reged, berminyak, utawa teyeng.Isi silikon dhuwur nambah fluidity saka blumbang weld, saéngga nggawe tampilan manik Gamelan lan asil ing minimal post-weld grinding.Kabel iki direkayasa kanggo nyedhiyakake welds kualitas sinar-x tanpa porositas kanthi kekuatan tarik paling dhuwur (minangka dilas) saka kabeh kabel baja karbon biasa.

Aplikasi Umum: aplikasi toko umum kanthi piring lengo utawa karat;casting baja utawa forging nyelametake;proyek ngarep;lembaran logam;tank;karya konstruksi

Kelas AWS: ER70S6

Sertifikasi: AWS A5.18/A5.18M:2005

Paduan: ER70S6

ASME SFA A5.18

Posisi Welding: F, V, OH, H

Saiki: DCEP

Kekuwatan tarik, kpsi:

70

Kekuwatan Ngasilake, kpsi:

58

Elongasi ing 2 "%:

22

Kimia Wire Khas miturut AWS A5.18 (nilai tunggal maksimal)

C

Mn

Si

P

S

Ni

Cr

Mo

V

Cu

0.06-0.15

1.40-1.85

0.80-1.15

0,025

0.035

0.15

0.15

0.15

0.03

0.50

Parameter Welding Khas

Dhiameter

Proses

Volt

Kacepetan Lelungan

Ampere

Gas pelindung

in

(mm)

(ipm)

.035

(0.9)

GMAW

23-26

11-22

160-300

Transfer Semprotan 98% Argon + 2% Oksigen

.045

(1.2)

GMAW

23-29

12-21

170-375

Transfer Semprotan 98% Argon + 2% Oksigen

1/16

(1.6)

GMAW

25-31

9-19

275-475

Transfer Semprotan 98% Argon + 2% Oksigen

.023

GMAW

14-19

10-15

30-85

Short Circuiting Transfer 98% Argon + 2% Oksigen

.030

(0.8)

GMAW

15-20

12-24

40-130

Short Circuiting Transfer 98% Argon + 2% Oksigen

.035

(0.9)

GMAW

16-25

11-40

60-235

Short Circuiting Transfer 98% Argon + 2% Oksigen

.045

(1.14)

GMAW

18-23

12-22

90-290

Short Circuiting Transfer 98% Argon + 2% Oksigen

.035

(0.9)

GTAW

12-15

N/A

60-100

100% Argon

.045

(1.14)

GTAW

13-16

N/A

70-120

100% Argon

1/16

(1.6)

GTAW

12

N/A

100-160

100% Argon

1/16- 3/32

(1.6)-(2.4)

GTAW

12

N/A

120-250

100% Argon

1/8

(3.2)

GTAW

12

N/A

150-300

100% Argon