Kawat las stainless steel nduweni efisiensi cladding sing dhuwur, kinerja teknis welding sing apik ing welding kabeh posisi.Padha digunakake digunakake ing industri: struktur bangunan, kendaraan, engineering jembatan, mesin pertambangan, railway, pipe lenga, gas meksa-prewangan peralatan, peralatan daya, etc.


Detail Produk

Tag produk

Klasifikasi AWS: AWS 5.9

DESKRIPSI:

Kawat las stainless steel nduweni efisiensi cladding sing dhuwur, kinerja teknis welding sing apik ing welding kabeh posisi.Digunakake sacara wiyar ing industri: struktur bangunan, kendaraan, teknik jembatan, mesin pertambangan, sepur, pipa minyak, peralatan bantalan tekanan gas, peralatan listrik, lsp.

MODEL NO.& UKURAN:

1. Pabrik pasokan layanan OEM.

2. Model: ER308 ER308L ER308LSi ER309 ER309L ER316 ER316L ER316LSi lsp.

3. ukuran kabel MIG: 0.8mm 0.9mm 1.0mm 1.2mm 1.6mm.

4. TIG ukuran kawat: 1.6mm 2.0mm 2.4mm 3.2mm 4.0mm.

PAMBUKA:

Kita nyedhiyakake macem-macem kawat las stainless steel, kalebu kawat las padat Mig, kawat las rod Tig lan kawat las busur submerged, kabeh kualitas dhuwur lan didol ing saindenging jagad.

Kajaba 308 lan 309, kita uga nawakake 304, 321, 347, 316L, 310, 2209, lan 201. Uga spesifikasi khusus kayata 318L, 904L, 2594, NiCrMo-3, Ni1.

PACKING:

Mig welding wire packing (spool and drum pack)

Dhiameter: 0.8 - 2.0mm

Paket: 1 kg/spool, 5 kg/spool, 15 kg/spool, 20 kg/spool, 100 kg/drum, 200 kg/drum

Tig rod welding wire packing (tabung plastik)

Dhiameter: 1.0 - 5.0mm

Paket: 5 kg/paket

Kawat las busur submerged

Dhiameter: 2.5 - 5.0mm

Paket: 20kg/pack, 25kg/pack

Kemasan netral lan OEM olèh!

KOMPOSISI KIMIA KAWAT LAS STAINLESS STEEL:

Model No.

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

304

0.08

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-11.00

0.18

0.003

304L

0.03

0.30-1.00

2.00

0.045

0.030

18.00-20.00

8.00-12.00

ER307

0.04-0.14

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

8.00-10.70

0.5-1.5

0.75

ER308

0.08

0.30-0.65

4.30-4.75

0.030

0.030

19.50-22.00

9.00-11.00

0.75

0.75

ER308L

0.03

0.30-0.65

1.50-2.30

0.03

0.02

19.5-21.5

9.00-11.00

0.75

0.75

ER308LSi

0.03

0.65-1.00

1.60-2.40

0.03

0.02

19.5-21.5

9.0-11.0

0.75

0.75

ER309

0.12

0.30-0.65

1.00-2.50

0.03

0.03

24.0-25.0

12.0-14.0

0.75

0.75

ER309L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER309LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

23.0-25.0

12.0-14.0

0.75

0.75

ER316

0.08

0.3-0.65

1.0-2.5

0.03

0.03

18.00-12.00

11.0-14.0

2.0-3.0

0.75

ER316L

0.03

0.3-0.65

1.5-2.3

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER316LSi

0.03

0.65-1.0

1.6-2.4

0.03

0.02

18.0-20.0

11.0-13.0

2.05-2.55

0.75

ER310

0.08-0.15

0.3-0.65

1.0-2.5

0.03

0.03

25.0-28.0

20.0-22.5

0.75

0.75

ER347

0.08

0.3-0.65

1.0-2.5

0.03

0.03

19.0-21.5

9.0-11.0

0.75

0.75

ER317

0.08

0.3-0.65

1.0-2.5

0.03

0.01

18.5-20.5

13.0-15.0

3.0-4.0

0.75

ER321

0.08

0.3-0.65

1.5-2.5

0.03

0.01

18.5-20.5

9.0-10.5

0.75

0.75

SIFAT MEKANIKAL KAWAT LAS:

Model No.

Kekuatan tarik Rm(Mpa)

Kekuwatan ngasilake Rel utawa Rp0,2 (Mpa)

Elongation

(%)

Model No.

Kekuatan tarik Rm(Mpa)

Kekuwatan ngasilake Rel utawa Rp0,2 (Mpa)

Elongation

(%)

304

550

--

25

ER309LSi

510

320

25

304L

510

--

25

ER316

510

320

25

ER307

590

350

25

ER316L

510

320

25

ER308

550

350

25

ER316LSi

510

320

20

ER308L

510

320

25

ER310

550

350

25

ER308LSi

510

320

25

ER347

550

350

25

ER309

550

350

25

ER317

550

350

25

ER309L

510

320

25

ER321

550

350

25

Komposisi kawat las baja tahan karat TIG lan MIG

YB5092-2005

AWS

Komposisi kimia %

C

Si

Mn

P

S

Cr

Ni

Mo

H08Cr20Ni9Mn7Si

ER307Si

0.075

0.78

6.7

0,022

0.01

19.8

8.8

H06Cr21Ni10

ER308

0.045

0.45

1.9

0.02

0.009

20.8

9.8

H0OCr21Ni10

ER308L

0.02

0.32

1.9

0.011

0.006

20

10.2

H06Cr21Ni10Si

ER308Si

0.045

0.85

1.5

0,022

0.01

20.8

9.8

H06Cr24Ni13

ER309

0.06

0.45

1.9

0.019

0.009

24.3

13.2

H06Cr24Ni13Si

ER309Si

0.06

0.79

1.95

0.019

0.009

24.7

13.2

H03Cr24Ni13

ER309L

0.02

0.42

1.8

0.02

0.01

24.8

13.2

H03Cr24Ni13Si

ER309LSi

0.018

0.8

1.7

0.02

0.01

23.5

13.5

H21Cr16Ni35

ER330

0.2

0.38

1.5

0,022

0.01

16.5

34.5

H06Cr19Ni12Mo2

ER316

0.04

0.4

1.9

0.02

0.01

19.5

11.8

2.3

H06Cr19Ni12Mo2Si

ER316Si

0.05

0.7

1.92

0.02

0.01

19.5

11.8

2.3

H03Cr19Ni12Mo2

ER316L

0.019

0.38

1.8

0.018

0.01

19.8

12.2

2.5

H03Cr19Ni12Mo2Si

ER316LSi

0.06

0.85

1.7

0,022

0.01

18.8

12.6

2.4

H03Cr17Ni14Mo3

ER317L

0.02

0.38

1.8

0.02

0.01

18.8

13.8

3.6

H08Cr19Ni12Mo2Nb

ER318

0.06

0.42

1.5

0,022

0.01

18.5

11.8

2.3

H07Cr20Ni34Mo2Cu3Nb

ER320

0.06

0.4

1

0,022

0.01

19.8

33.3

2.8

Nb0.7

H02Cr20Ni34Mo2Cu3Nb

ER320L

0.018

0.33

1.5

0.013

0.01

19.8

33.6

2.5

Nb0.35

H08Cr20Ni10Ti

ER321

0.06

0.45

1.5

0,022

0.01

20.8

9.8

Ti9xC-1.0

H08Cr21 Ni10Nb

ER347

0,055

0.48

1.8

0,021

0.008

20.8

9.8

Nb1xC-1.0

H12Cr26Ni21

ER310

0.09

0.5

1.66

0.02

0.01

25.5

20.5

H02Cr20Ni25Mo4Cu

ER385

0.02

0.3

1.5

0.018

0.01

20.2

24.8

4.8

Cu 1,80

H03Cr22Ni9Mo3N

ER2209

0,022

0.5

0.9

0.02

0.01

22.5

8.8

3.3

N0.08-0.20

H04Cr25Ni5Mo3Cu2N

ER2553

0,027

0.5

1

0,025

0.015

24.8

5.5

3.2

N0.1-0.25

H1 5Cr29Ni9

ER312

0.09

0.38

1.5

0,022

0.01

29.5

8.5

H03Cr24Ni13MoL

ER309L Mo

0,023

0.45

1.5

0,022

0.01

23.8

13.2

2.2

H05Cr17Ni4Cu4Nb

ER630

0.04

0.39

0.5

0,022

0.01

16.5

4.8

Cu;3 Nb;0.28

H08Cr26Ni5Mo2

ER453s

0.06

0.3

0.4

0,022

0.01

25.8

4.8

2.1

H08Cr21Ni10Mn6

0.06

0.35

5.5

0,022

0.01

20.8

9.8

H05Cr22Ni11Mn6Mo3VN

ER209

0.04

0.4

4.5

0,022

0.01

21.5

10.8

2.2

N;0.20 V;0.18

Wenzhou Tianyu Electronic Co., Ltd. didegaké ing taun 2000. Kita wis melu manufaktur elektroda welding, rod welding, lan bahan welding luwih saka 20 taun.

Produk utama kami meliputi elektroda las stainless steel, elektroda las baja karbon, elektroda las paduan rendah, elektroda las permukaan, elektroda las paduan nikel & kobalt, kawat las baja ringan & paduan rendah, kabel las stainless steel, kabel inti fluks terlindung gas, kabel las aluminium, las busur submerged.kabel, kabel las nikel & kobalt paduan, kabel las kuningan, kabel las TIG & MIG, elektroda tungsten, elektroda gouging karbon, lan aksesoris las liyane & consumables.

 

Wenzhou Tianyu Electronic Co., Ltd. didegaké ing taun 2000. Kita wis melu manufaktur elektroda welding, rod welding, lan bahan welding luwih saka 20 taun.

Produk utama kami meliputi elektroda las stainless steel, elektroda las baja karbon, elektroda las paduan rendah, elektroda las permukaan, elektroda las paduan nikel & kobalt, kawat las baja ringan & paduan rendah, kabel las stainless steel, kabel inti fluks terlindung gas, kabel las aluminium, las busur submerged.kabel, kabel las nikel & kobalt paduan, kabel las kuningan, kabel las TIG & MIG, elektroda tungsten, elektroda gouging karbon, lan aksesoris las liyane & consumables.


  • Sadurunge:
  • Sabanjure: