AWS ER5183 Aluminium Welding Wire Aluminium MIG Welding Rods Tig Wire

Katrangan singkat:

ER5183 cocok kanggo MIG welding aluminium Magnesium alloy sing kekuatan tensile luwih dibutuhake lan yen basa logam punika 5083 utawa 5654 kekuatan tensile bakal luwih.Iki digunakake digunakake kanggo welding struktur aluminium alloy Magnesium kapal, platform lepas pantai, lokomotif & gerbong, kendaraan motor, kontaner, prau cryogenic lan ing.


Detail Produk

Tag produk

ER5183 cocok kanggo MIG welding aluminium Magnesium alloy sing kekuatan tensile luwih dibutuhake lan yen basa logam punika 5083 utawa 5654 kekuatan tensile bakal luwih.Iki digunakake digunakake kanggo welding struktur aluminium alloy Magnesium kapal, platform lepas pantai, lokomotif & gerbong, kendaraan motor, kontaner, prau cryogenic lan ing.logam weld sawijining wis resistance apik kanggo brine karat.

Posisi Welding: F, HF, V

Tipe Arus: DCEP

WARTA:

Njaga paket kabel ing kondisi apik sadurunge welding.

Loro-lorone lumahing sing bakal dilas saka weldment lan kabel kudu di resiki adoh impurities saka kontaminasi lenga, lapisan oksida, Kelembapan lan ing.

Kanggo entuk tampilan weld sing apik, preheat logam dhasar nganti 100 ℃ -200 ℃ sadurunge welding yen kekandelane 10mm utawa luwih.

Iku luwih apik kanggo nyelehake subplate ing zona weld kanggo nyonggo logam ilang supaya kanggo mesthekake seng nembus lengkap weldment.

Miturut posisi welding lan kekandelan saka logam dhasar beda gas tameng kudu milih, kayata 100% Ar, 75% Ar + 25% He, 50% Ar + 50% He, etc.

Kondisi welding kasebut ing ndhuwur mung kanggo referensi lan luwih apik kanggo nindakake kualifikasi prosedur welding miturut project sadurunge sijine menyang welding formal.

ER5183 KOMPOSISI KIMIA LOGAM SIMPANAN (%):

SI FE CU MN MG CR ZN TI AI BE
Standar ≤0.40 ≤0.40 ≤0.10 0.50-10 4.3-52 0.05-0.5 ≤0.25 ≤0.15 imbangan ≤0,0003
Khas 0.08 0.12 0.006 0.65 4.75 0.130 0.005 0.080 imbangan 0.0001

SIFAT MEKANIKAL LOGAM DEPOSIT (AW):

KEKUATAN TENSI RM (MPA) REL KEKUATAN PENGHASILAN (MPA) ELONGASI A4 (%)
Khas 280 150 18

Ukuran & Arus sing Disaranake kanggo MIG (DC+):

DIAMETER KABEL LAS (MM) 1.2 1.6 2.0
Arus Las (A) 180-300 200-400 240-450
Tegangan Las (V) 18-28 20-20 22-34

UKURAN & REKOMENDASI ​​SAIKI UNTUK TIG (DC¯):

DIAMETER KABEL LAS (MM) 1.6-2.5 2.5-4.0 4.0-5.0
Arus Las (A) 150-250 200-320 220-400