AWS ERNiCrMo-7 Nikel Alloy Welding Wire Mig and Tig Wire, Arc Welding Rods Pemasok Welding Terbaik

Katrangan singkat:

ERNiCrMo-10 digunakake kanggo ngelas bahan dasar nikel-kromium-molybdenum kanggo awake dhewe, baja lan paduan basa nikel liyane, lan kanggo baja cladding.Bisa digunakake kanggo las duplex, baja tahan karat super duplex.


Detail Produk

Tag produk

DESKRIPSI PRODUK:

AWS: A5.14

Sesuai karo Sertifikasi: AWS A5.14 ASME SFA A5.14

Proses Las: Proses Pengelasan GMAW & ASAW

ERNiCrMo-10 digunakake kanggo ngelas bahan dasar nikel-kromium-molybdenum kanggo awake dhewe, baja lan paduan basa nikel liyane, lan kanggo baja cladding.Bisa digunakake kanggo las duplex, baja tahan karat super duplex.

Syarat Komposisi Kimia AWS

C = 0,015 maks Cu = 0,50 maks
Mn = 1,0 maks Ni = Sisa
Fe = 3,0 maks Co = 2,0 maks
P = 0,04 maks Cr = 14,0 - 18,0
S = 0,03 maks Mo = 14,0 - 18,0
Si = 0,08 maks W = 0,50 maks
Liyane = 0,50 maks Ti = 0,70 maks

Mangga nelpon kanggo informasi luwih lengkap lan ukuran kasedhiya:

Aplikasi

ERNiCrMo-7 digunakake kanggo welding bahan dasar nikel-kromium-molybdenum kanggo awake dhewe, baja lan wesi basa nikel liyane lan kanggo cladding baja karo bahan las NI-CR-MO.

PARAMETER PRODUK:

Komposisi Kimia sing Disimpen % (Khas)
C = 0,01 Cr = 16,5 Ni = imbangan
Fe = 2,20 Mo = 15,75
Setor Kabeh Sifat Logam Las % (AW)
Kekuwatan Tensile 113,00 psi
Elongation 29%

SIFAT DAMPAK CHARPY-V-NOTCH sing disimpen:

Ora ditrapake

Parameter Welding Dianjurake kanggo MIG lan SAW Welding saka Nikel Alloys
Proses Diameter Kawat Tegangan (V) Ampere (A) Gas
MIG .035 in 26 - 29 150 - 190 75 % Argon + 25% Helium
.045 ing 28 - 32 180 - 220 75 % Argon + 25% Helium
1/16 inchi 29 - 33 200 - 250 75 % Argon + 25% Helium
SAW 3/32 in 28 - 30 270 - 350 Fluks sing cocog Bisa Digunakake.
1/8 inchi 29 - 32 350 - 450 Fluks sing cocog Bisa Digunakake.
5/32 inchi 30 - 33 400 - 550 Fluks sing cocog Bisa Digunakake.