H10MnSi AWS EM13K Submerged Arc Welding Wire

Katrangan singkat:

H10MnSi Kawat las busur submerged yaiku jinis kawat las jinis medium mangan lan silikon.


Detail Produk

Tag produk

H10MnSi AWS EM13K Submerged Arc Welding Wire

EM13K 2.5/3.2/4.0/5.0mm Submerged Arc Welding Wire

H10MnSi Kawat las busur submerged yaiku jinis kawat las jinis medium mangan lan silikon.
1. Iku cocog karo medium-mangan lan medium-silikon jinis welding flux.
2. Iku ora sensitif teyeng ing logam dhasar.
3. Wis banget manik ngecor lan slag detachability.
4. Monopole utawa dipole.AC DC.
5. Iki digunakake kanggo welding kacepetan dhuwur lan welding ngisi ing logam dasar kelas 50kg.
6. welding liyane 501 Mpa baja karbon tingkat lan baja alloy kurang

EM13K Selaras karo Standar:GB/T 5293 H10MnSi
AWS EM13K
ISO 14171-B-SU25

Spesifikasi: Iki minangka jinis kawat las kanthi konten mangan lan silikon sing cocog., Cocog karo fluks las jinis mangan rendah lan silikon, Ora sensitif marang karat ing logam dasar.Nduwe cetakan manik sing apik, kemampuan nyopot slag sing apik.

Tujuan: Nggunakake karo fluks sintered LT.SJ101, bisa Applied loro kanggo dhuwur-kacepetan welding steel plate kekuatan tensile 420N/mm2 lan Isi welding.Kang digunakake digunakake kanggo welding boiler, prau meksa, jembatan, kapal etc.

Komposisi kimia (%)

 

 

Komposisi kimia C Mn Si S P Cr Ni Cu
Nilai njamin ≤0.14 0.80~
1.10
0.60~
0.90
≤0,035 ≤0,035 ≤0.20 ≤0.30 ≤0.35
Hasil Umum 0.089 0.98 0.67 0,023 0.032 0.015 0.034 0.11

 
Sifat-sifat Mekanik Logam Setor

Item tes

Fluks

Rm (MPa) ReL/Rp0.2(MPa) A(%) KV2(J)
-20 ℃
LT•SJ101 415~550 ≥330 ≥22 ≥27

 
Ukuran Welding Wire

Ukuran (mm) Φ2.5 Φ3.2 Φ4.0 Φ5.0

 