Hardfacing Welding Electrode Surfacing Welding Rods DIN 8555 (E10-UM-60-GRZ) Stick Electrode kanggo Arc Welding

Katrangan singkat:

DIN 8555 (E10-UM-60-GRZ) punika elektroda SMAW Recovery dhuwur ditutupi dhasar kanggo hardsurfacing.


Detail Produk

Tag produk

Hardfacing WeldingElektroda

 

Standar: DIN 8555 (E10-UM-60-GRZ)

Tipe No.: TY-C LEDURIT 61

 

Spesifikasi & Aplikasi:

· Dasar ditutupi elektroda SMAW Recovery dhuwur kanggo hardsurfacing.

· Lumahing ekstra hard saka bagean ngalami abrasion abot lan impact Moderate.

· Cocog kanggo lapisan hard final sawise lapisan buffer.

· Bagean tanduran Sinter, nyandhang bar lan piring, scraper bar, blast furace, sistem daya, tungku semen, untu ember lan lambé, layar.

 

Komposisi kimia saka logam setor (%):

 

C

Si

Mn

Cr

Mo

Nb

W

V

Ni

Fe

DIN

Isi C lan Cr dhuwur

Bal.

EN

1.5

4.5

-

0.5

3.0

25

40

-

4.0

-

-

-

-

4.0

Bal.

Khas

3.2

1.0

1.8

29

-

-

-

-

-

Bal.

 

 

Kekerasan logam sing disimpen:

Minangka Welded

(HRC)

1 lapisan ing baja karo C = 0,15%

(HRC)

1 lapisan ing dhuwur Mn-baja

(HRC)

60

55

52

 

Karakteristik Umum:

· Struktur Mikro Martensit + Austenit + Karbida

· Machinability Grinding mung

· Redrying Redry kanggo 2 jam ing 300 ℃ sadurunge nggunakake.

 


  • Sadurunge: